Heat Shrink Tubing

Compare part numbers, manufacturers and available catalog specifications. Open a product for complete details, pricing and availability.

  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.5 in
    Recovered Inner Diameter
    0.25 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.025 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.25 in
    Recovered Inner Diameter
    0.125 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.125 in
    Recovered Inner Diameter
    0.062 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.035 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    1 in
    Recovered Inner Diameter
    0.5 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.045 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    2 in
    Recovered Inner Diameter
    1 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.045 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    2 in
    Recovered Inner Diameter
    1 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.045 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    2 in
    Recovered Inner Diameter
    1 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.045 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    2 in
    Recovered Inner Diameter
    1 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.045 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    2 in
    Recovered Inner Diameter
    1 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.045 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    2 in
    Recovered Inner Diameter
    1 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.093 in
    Recovered Inner Diameter
    0.046 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Red
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    White
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Yellow
    Wall Thickness
    0.03 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.75 in
    Recovered Inner Diameter
    0.375 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.016 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.046 in
    Recovered Inner Diameter
    0.023 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.016 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.046 in
    Recovered Inner Diameter
    0.023 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.02 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.187 in
    Recovered Inner Diameter
    0.093 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Black
    Wall Thickness
    0.016 in
    Resistance Properties
    Corrosion Resistant, Microbial Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.046 in
    Recovered Inner Diameter
    0.023 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.016 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.046 in
    Recovered Inner Diameter
    0.023 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Blue
    Wall Thickness
    0.016 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.046 in
    Recovered Inner Diameter
    0.023 in
    Recovery Temperature
    121 °C
  • Material
    Cross-Linked Polyolefin
    Color
    Green
    Wall Thickness
    0.016 in
    Resistance Properties
    Corrosion Resistant, Fluid Resistant, Microbial Resistant, Water Resistant
    Shrink Ratio
    2:1
    Operating Temperature
    -55 to 135 °C
    More specifications (4)
    Dielectric Strength
    500 V/mil
    Expanded Inner Diameter
    0.046 in
    Recovered Inner Diameter
    0.023 in
    Recovery Temperature
    121 °C